ALTECH PA6 A 4020/100 MR20
General | |
Material Status | Commercial: Active |
Availability | Asia PacificEuropeNorth America |
Filler / Reinforcement | Mineral Filler, 20% Filler by Weight |
Additive | Heat Stabilizer |
Features | Heat StabilizedHigh FlowHigh Impact ResistanceHigh RigidityHigh StrengthLow Warpage |
Uses | Housings |
Processing Method | Injection Molding |
ALTECH PA6 A 4020/100 MR20 及其它型号:
ALTECH PA6 1461 Z 2 ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 100/520 UV HV ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/107 ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/108 ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/109 ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/110 IM ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/120 UV ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/126 UV ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/149 FR ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/310 IM ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/316 IM ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/506 HV ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/510 IM ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/518 IM ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/586 ALBIS PLASTIC GmbH Nylon 6
ALTECH PA6 A 1000/700 ALBIS PLASTIC GmbH Nylon 6
加工工艺
融化温度:
230-280℃,对于增强品种为250-280℃。
模具温度:
80-90℃。模具温度很显著地影响结晶度,而结晶度又影响着塑件的机械特性。对于结构部件来说结晶
度很重要,因此建议模具温度为80-90℃。对于薄壁的、流程较长的塑件也建议施用较高的模具温度。增
大模具温度可以提高塑件的强度和刚度,但却降低了韧性。如果壁厚大于3mm,建议使用20-40℃的低温
模具。对于玻璃纤维增强材料模具温度应大于80℃。
ALTECH PA6 A 4020/100 MR20 价格优惠,质量保证。
ALTECH PA6 A 4020/100 MR20 原材料产地证明 SGS,MSDS.UL黄卡
ALTECH PA6 A 4020/100 MR20 东莞市艾博(国际)塑胶进口出口有限公司现货供应 PA6 全系列产品可随货提供原材料物性,原材料产地证明SGS.MSDS.UL黄卡等相关详细资料,可开具17%增值税发票.公司秉着“以诚为本,以信为用”的经营理念。与客户是建立在互惠、互利、互信的基础上长期合作。共创双赢局面,愿与各界人士真诚合作,共同发展,携手共创辉煌的明天.
欢迎来人来电咨询洽谈:
直线:0769-88038808
传真:0769-88768175
邓小姐:13728215822
E-mail:abba2010@163.com
网址:www.abplas.com.cn