原厂原包美国道康宁TPSiV 3451-80A包胶级
原厂原包美国道康宁TPSiV 3451-80A包胶级
Density |
1.20 |
g/cm? |
ISO 1183 |
Spiral Flow2 |
28.0 |
cm |
Internal Method |
Hardness | Nominal Value |
Unit |
Test Method |
Shore Hardness(Shore A) |
84 |
ISO 868 |
Mechanical | Nominal Value |
Unit |
Test Method |
Tensile Stress |
ISO 527-2/5A/50 | ||
Break |
9.10 |
MPa |
|
*** Strain |
5.70 |
MPa |
|
Tensile Strain(Break) |
350 |
% |
ISO 527-2/5A/50 |
Elastomers | Nominal Value |
Unit |
Test Method |
Tear Strength |
50 |
kN/m |
ISO 34-1 |
Injection | Nominal Value |
Unit |
|
Drying Temperature - Desiccant Dryer |
80 to 100 |
°C |
|
Drying Time - Desiccant Dryer |
3.0 to 6.0 |
hr |
|
Suggested Max Moisture |
0.030 |
% |
|
Rear Temperature |
180 to 190 |
°C |
|
Middle Temperature |
200 to 210 |
°C |
|
Front Temperature |
205 to 215 |
°C |
|
Nozzle Temperature |
210 to 220 |
°C |
|
Processing (Melt) Temp |
215 |
°C |
|
Mold Temperature |
10 to 40 |
°C |
|
Back Pressure |
0.700 to 1.40 |
MPa |
|
Screw Speed |
100 to 150 |
rpm |
|
Vent Depth |
0.013 to 0.025 |
mm |
与一般热塑性弹性体 TPE、TPV、TPU合金等相比,有机硅弹性体 TPSiV 具有更好的拉伸和撕裂强度,更好的
***耗和产品保护,高温下更好的压缩弹性形变,更加***的粘接强度(与 PC、PA、ABS、PVC等),更好的抗UV性能和耐
热性能。 TPSiV 与 EPDM/TPV、
TPU/SEBS合金两种弹性体材料的物理机械性能,与 PC的粘接强度,***耗性能,压缩弹性形变,抗 UV 性能
(0.5W/m2@340nm, 500h),耐热性( 120 ℃热空气 /1000h )的对比:
TPSiV 材料的应用发展
随着科学技术的飞速发展和社会文明的不断进步,人们在对健康生活品质的要求不断提高的同时,也更加重视周围环境的可
持续发展问题。绿色、环保、清洁***也是高分子材料未来发展的趋势。为此,在不断提高现有机硅弹性体 TPSiV 材
料性能的同时,也在积极开发新的有机硅弹性体 TPSiV 市场的需求: