江苏普及塑料有限公司
牌号简介About |
---|
(PC+ABS)混合物;未增强;阻燃;注塑等级;VICAT/B 120温度=99°C;UL识别94 V-0(1.0 mm);热线测试(GWFI):960°C(2.0 mm);用于笔记本和薄壁应用。 (PC+ABS)-Blend; flame retardant; Vicat/B 120 temperature = 99°C; UL recognition 94 V-0 (1.0 mm); glow wire temperature (GWFI): 960°C at 2.0 mm; for notebooks and thinwall applications |
产品描述Product Description
厂家:德国科思创Covestro - PUR
类别:PC+ABSPC+ABS
用途:薄壁部件;
加工条件:注射成型Injection Molding
性能特点:阻燃;Flame Characteristics
技术参数Technical Data | |||
---|---|---|---|
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
密度Specific Gravity | 1.18 | g/cm3 | ISO 1183 |
收缩率Molding Shrinkage | |||
MD:2.0 mmMD2.0mm | 0.60 | % | ISO 294-4 |
TD:2.0 mmTD2.0mm | 0.60 | % | ISO 294-4 |
吸水率Water Absorption | |||
23℃,24hr(23°C, 24 hr) | 0.50 | % | ISO 62 |
23℃,50% RH(23°C, 50RH) | 0.20 | % | ISO 62 |
熔体质量流动速率熔融流动指数 | |||
240℃,5.0kg240℃ / 5.0Kg | 19 | g/10min | ISO 1133 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
拉伸强度拉伸强度 | |||
23℃23°C | 60 | MPa | ISO 527-2 |
拉伸应变Tensile Elongation at Break | |||
断裂,23℃23°C | 50 | % | ISO 527-2 |
拉伸模量Tensile Modulus | |||
23℃23°C | 2700 | MPa | ISO 527-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
热变形温度Heat Deflection Temperature | |||
0.45 MPa,未退火0.45MPa 未退火 | 92 | ℃ | ISO 75-2/Bf |
1.8 MPa,退火1.80MPa 退火 | 84 | ℃ | ISO 75-2/Af |
维卡软化温度Vicat Softening Temperature | |||
B50 | 97 | ℃ | ISO 306 |
线性热膨胀系数线膨胀系数 | |||
MDMD | 7.6E-5 | 1/℃ | ISO 11359-2 |
TDTD | 8.0E-5 | 1/℃ | ISO 11359-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
体积电阻体积电阻 | 1.0E+16 | Ω.cm | IEC 60093 |
表面电阻表面电阻 | 1.0E+16 | Ω.cm | IEC 60093 |
绝缘强度绝缘强度 | |||
35 | KV/mm | IEC 60243-1 | |
介电常数Dielectric Constant | |||
23℃23°C | 3.10 | 1 MHz | IEC 60250 |
耗散因数Dissipation Factor | |||
23℃ 23°C | 6.0E-3 | 1 MHz | IEC 60250 |
相比漏电起痕指数相对漏电起痕指数 | 300 | V | IEC 60112 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
阻燃等级防火等级 | |||
0.75mm | UL 94 | ||
0.90mm | V-0 | UL 94 | |
1.00mm | V-0 | UL 94 | |
1.50mm | V-0 | UL 94 | |
1.80mm | V-0,5VB | UL 94 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
悬臂梁缺口冲击强度Notched Izod Impact Strength | |||
23℃23°C | 30 | kJ/m2 | ISO 180-1A |