东莞市常平嘉美塑胶原料贸易行
TPV SARLINK X6155N
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.910g/cc | 0.0329lb/in3 | ISO 1183 |
Viscosity | 215cP @Shear Rate 206 1/s, Temperature 200 °C |
215cP @Shear Rate 206 1/s, Temperature 392 °F |
Shear, Capillary; ASTM D3835 |
Mechanical Properties | Metric | English | Comments |
Hardness, Shore A | 53 @Time 5.00 sec |
53 @Time 0.00139 hour |
Extruded; ISO 868 |
58 @Time 5.00 sec |
58 @Time 0.00139 hour |
Injection Molded; ISO 868 | |
Tensile Strength at Break | 3.40MPa | 493psi | Flow; ISO 37 |
4.39MPa | 636psi | Across Flow; ISO 37 | |
Tensile Strength | 1.80MPa @Strain 100 % |
261psi @Strain 100 % |
Across Flow; ISO 37 |
2.40MPa @Strain 100 % |
348psi @Strain 100 % |
Flow; ISO 37 | |
Elongation at Break | 340 % | 340 % | Flow; ISO 37 |
610 % | 610 % | Across Flow; ISO 37 | |
Tear Strength | 21.0kN/m | 120pli | Method Ba, Angle (Unnicked); ISO 34-1 |
TPV SARLINK X6155N
TPV是Thermoplastic Vulcanizate的简称,中文名称为热塑性三元乙丙动态硫化弹性体或热塑性三元乙丙动态硫化橡胶,是高度硫化的三元乙丙橡胶EPDM微粒分散在连续聚丙烯PP相中组成的高分子弹性体材料。TPV常温下的物理性能和功能类似于热固性橡胶,在高温下表现为热塑性塑料的特性,可以快速经济和方便地加工成型。TPV热塑性三元乙丙动态硫化弹性体/橡胶将硫化橡胶材料通过动态硫化使三元乙丙橡胶EPDM以低于2微米尺寸的微粒分散在聚丙烯PP塑料基体中,把橡胶与塑料的特性很好的结合在一起,得到综合性能优异的高性能弹性体材料。
性能:
1、良好的弹性和耐压缩变形性,耐环境、耐老化性相当于三元乙丙橡胶,同时其耐油耐溶剂性能与通用型氯丁橡胶不相上下。
2、应用温度范围广(– 60—150℃),软硬度应用范围广(25A—54D),易染色的优点大大提高了制品设计的自由度。
3、优良的加工性能:可用注射、挤出等热塑性塑料的加工方法加工,高效、简单易行,无需增添设备,流动性高、收缩率小。
4、绿色环保,可回收使用,且反复使用六次性能无明显下降,符合欧盟环保要求。
5、比重轻(0.90—0.97),外观质量均匀,表面档次高,手感好。
电子电器
1、各种耳机线外皮,耳机线接头;
2、矿山电缆、数控同轴电缆、普通及高档电线电缆绝缘
层及护套;
3、电源插座、插头与护套等;
4、电池、无线电话机外壳及电子变压器外壳护套;
5、船舶、矿山、钻井平台、核电站及其它设施的电力电缆线的绝缘层及护套。