技术参数Technical Data | |||
---|---|---|---|
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
密度Specific Gravity | 1.20 | g/cm3 | ASTM D792 |
特定体积Specific Volume | 0.830 | cm3/g | ASTM D792 |
密度Density | 1.19 | g/cm3 | ASTM D792 |
熔体质量流动速率熔体质量流动速率 | |||
300℃,1.20kg300℃/1.2 kg | 18 | g/10min | ASTM D1238 |
熔体体积流动速率熔体体积流动速率 | |||
300℃,1.2 kg300℃/1.2 kg | 16.0 | cm3/10min | ISO 1133 |
收缩率收缩率 | |||
MD:3.2 mmMD,3.20 mm | 0.50 to 0.70 | % | 内部方法 |
吸水率Water Absorption | ASTM D570 | ||
24hr24 hr | 0.15 | % | ASTM D570 |
平衡,23℃Equilibrium, 73°F | 0.35 | % | ASTM D570 |
平衡,100℃Equilibrium, 212°F | 0.58 | % | ASTM D570 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
简支梁缺口冲击强度简支梁缺口冲击强度 | |||
23℃23℃ | 35 | kJ/m2 | ISO 179/2C |
悬臂梁缺口冲击强度Notched Izod Impact Strength 77 | ISO 180/1A | ||
23℃23℃ | 690 | J/m | ASTM D256 |
23℃23℃ | 3200 | J/m | ASTM D4812 |
-30℃-30°C | 10 | kJ/m2 | ISO 180-1A |
23℃23°C | 12 | kJ/m2 | ISO 180-1A |
装有测量仪表的落镖冲击装有测量仪表的落镖冲击 | |||
23℃,Energy at Peak Load23℃,Energy at Peak Load | 62.0 | J | ASTM D3763 |
落锤冲击落锤冲击 | |||
23℃23℃ | 169 | J | ASTM D3029 |
拉伸冲击强度Tensile Impact Strength 88 | 546 | kJ/m2 | ASTM D1822 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
热变形温度热变形温度9 | |||
1.8 MPa,未退火,6.4 mm1.8 MPa,未退火,6.40 mm | 129 | ℃ | ASTM D648 |
1.8 MPa,未退火,100 mm跨距1.8 MPa,未退火,100 mm Span9 | 122 | ℃ | ISO 75-2/Ae |
0.45 MPa,未退火,6.4 mm0.45 MPa,未退火,6.40 mm | 137 | ℃ | ASTM D648 |
0.45 MPa,未退火,100 mm跨距0.45 MPa,未退火,100 mm Span9 | 133 | ℃ | ISO 75-2/Be |
维卡软化温度Vicat Softening Temperature | 154 | ℃ | ASTM D1525 10 |
维卡软化温度Vicat Softening Temperature | |||
B50-- | 140 | ℃ | ISO 306 |
B120-- | 141 | ℃ | ISO 306/B120 |
球压测试球压测试 | |||
125℃125℃ | Pass | IEC 60695-10-2 | |
线性热膨胀系数线性热膨胀系数 | |||
MD:23~80℃MD:23 到 80℃ | 7.0E-5 | 1/℃ | ISO 11359-2 |
MD:-40~95℃MD:-40 到 95℃ | 6.8E-5 | 1/℃ | ASTM E831 |
比热Specific Heat | 1250 | J/kg/℃ | ASTM C351 |
导热系数Thermal Conductivity | 0.19 | W/m/K | ASTM C177 |
导热系数Thermal Conductivity | 0.20 | W/m/K | ISO 8302 |
相对温度指数相对温度指数 | |||
电气性能电气性能 | 130 | ℃ | UL 746 |
强度机械性能强度机械性能 | 130 | ℃ | UL 746 |
冲击机械性能冲击机械性能 | 130 | ℃ | UL 746 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
表面电阻率Surface Resistivity | 1.0E+15 | ohms | IEC 60093 |
体积电阻率Volume Resistivity | 1.0E+17 | ohms·cm | ASTM D257 |
体积电阻率Volume Resistivity | 1.0E+15 | ohms·cm | IEC 60093 |
介电强度介电强度 | |||
3.2 mm,在空气中3.20 mm,在空气中 | 15 | kV/mm | ASTM D149 |
3.2 mm,在油中3.20 mm,在油中 | 17 | kV/mm | IEC 60243-1 |
介电常数Dielectric Constant | ASTM D150 | ||
50 Hz50 Hz | 3.17 | ASTM D150 | |
60 Hz60 Hz | 3.17 | ASTM D150 | |
1 MHz1 MHz | 2.96 | ASTM D150 | |
相对电容率Relative Permittivity | IEC 60250 | ||
50 Hz50 Hz | 2.70 | IEC 60250 | |
60 Hz60 Hz | 2.70 | IEC 60250 | |
1 MHz1 MHz | 2.70 | IEC 60250 | |
耗散因数Dissipation Factor | ASTM D150 | ||
50 Hz50 Hz | 9.0E-4 | ASTM D150 | |
60 Hz60 Hz | 9.0E-4 | ASTM D150 | |
1 MHz1 MHz | 0.010 | ASTM D150 | |
耗散因数Dissipation Factor | IEC 60250 | ||
50 Hz50 Hz | 1.0E-3 | IEC 60250 | |
60 Hz60 Hz | 1.0E-3 | IEC 60250 | |
1 MHz1 MHz | 0.010 | IEC 60250 | |
相比漏电起痕指数Comparative Tracking Index (CTI) | PLC 2 | UL 746 | |
高电弧燃烧指数(HAI)High Amp Arc Ignition (HAI) | PLC 1 | UL 746 | |
高电压电弧起痕速率高电压电弧起痕速率 | |||
HVTRHVTR | PLC 2 | UL 746 | |
热丝引燃热丝引燃 | |||
HWIHWI | PLC 2 | UL 746 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
阻燃等级1.5 mm | |||
1.50 mm | HB | UL 94 | |
极限氧指数Oxygen Index | 25 | % | ISO 4589-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
折射率Refractive Index | 1.586 | ASTM D542 | |
透光率透射率 | |||
2540 μm2540 μm | 88.0 | % | ASTM D1003 |
雾度雾度 | |||
2540 μm2540 μm | 1.0 | % | ASTM D1003 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
拉伸模量Tensile Modulus 22 | 2370 | MPa | ASTM D638 |
拉伸模量Tensile Modulus | 2350 | MPa | ISO 527-1-2 |
拉伸强度拉伸强度3 | |||
断裂断裂3 | 68.0 | MPa | ASTM D638 |
断裂断裂 | 65.0 | MPa | ISO 527-2/50 |
屈服屈服 | 63.0 | MPa | ISO 527-2/50 |
屈服屈服3 | 62.0 | MPa | ASTM D638 |
拉伸应变拉伸应变 | |||
断裂断裂4 | 130 | % | ASTM D638 |
断裂断裂 | 100 | % | ISO 527-2/50 |
屈服屈服3 | 7.0 | % | ASTM D638 |
屈服屈服 | 6.0 | % | ISO 527-2/50 |
弯曲模量Flexural Modulus 55 | 2300 | MPa | ISO 178 |
50 mm跨距50.0 mm 跨距4 | 2340 | MPa | ASTM D790 |
弯曲强度Flexural Stress 5 ,65 ,6 | 90.0 | MPa | ISO 178 |
弯曲强度弯曲强度4 | |||
屈服,50 mm跨度屈服,50.0 mm 跨距4 | 96.0 | MPa | ASTM D790 |
泰伯耐磨性泰伯耐磨性 | |||
1000 周期,1000 g,CS-17 转轮1000 周期,1000 g,CS-17 转轮 | 10.0 | mg | ASTM D1044 |
洛氏硬度Rockwell Hardness | ASTM D785 | ||
M 级M-Scale | 70 | ASTM D785 | |
R 级R-Scale | 118 | ASTM D785 |