- 特性:增强
- 用途:纤维
- 加工方法:暂无
参数:密度:1.28g/cm3 熔指:4.8g/10 min 熔体体积流动速率:4.20cm3/10min 收缩率:0.20到0.40% 收缩率:0.050到0.20%
Iupilon? ABS/PC MB8900 耐冲击 高流动 Mitsubishi Engineering-Plastics Corp
Iupilon? PC ML-200 中等粘性 Mitsubishi Engineering-Plastics Corp
Iupilon? PC ML-300 低粘度 Mitsubishi Engineering-Plastics Corp
Iupilon? PC ML-400 高粘度 高流动 Mitsubishi Engineering-Plastics Corp
Iupilon? PC N-9 挤出级 阻燃级 Mitsubishi Engineering-Plastics Corp
Iupilon? PC RS-1001R 抗辐射 Mitsubishi Engineering-Plastics Corp
Iupilon? PC RS-3001R 抗辐射 Mitsubishi Engineering-Plastics Corp
Iupilon? PC S-1000 高粘度 Mitsubishi Engineering-Plastics Corp
Iupilon? PC S-2000 中等粘性 Mitsubishi Engineering-Plastics Corp
Iupilon? PC S-3000 低粘度 Mitsubishi Engineering-Plastics Corp
Iupilon? ABS/PC TMB1412 高刚度 Mitsubishi Engineering-Plastics Corp
Iupilon? ABS/PC TMB1615 高刚度 Mitsubishi Engineering-Plastics Corp
EVATHENE EVA UE633 挤出涂层用 注射成型 流动率20 VAC含量19 USI Corporation
EVATHENE EVA UE634-04 热稳定 高弹性 电线电缆应用 流动率6 VAC含量28 USI Corporation
EVATHENE EVA UE638-04 热稳定 高弹性 流动率18 VAC含量28 USI Corporation
EVATHENE EVA UE639-04 涂层应用 无纺布用 流动率150 VAC含量28 USI Corporation
EVATHENE EVA UE647-04 涂层应用 热稳定 高弹性 流动率800 VAC含量28 USI Corporation
EVATHENE EVA UE649-04 抗结块 热稳定 高弹性 流动率400 VAC含量19 USI Corporation
EVATHENE EVA UE653-04 食品级 包装用 粘合剂用 高弹性 流动率400 VAC含量28 USI Corporation
EVATHENE EVA UE654-04 电线电缆应用 良好粘结性 高弹性 流动率30 VAC含量32 USI Corporation
EVATHENE EVA UE659 高透明 耐低温冲击 高抗应力开裂 挤出级 流动率2 VAC含量25 硬度32D USI Corporation?