东莞市高创塑胶原料有限公司
Property
單位Unit
試驗方法TestMethod
試驗條件TestCondition
K9017
熔融指數MeltFlowIndex
g/10min
ASTMD-1238
230℃×2.16Kg
17
降伏點抗張強度TensileStrengthatYield
kg/cm2
ASTMD-638
23℃
210
斷裂點延伸率TensileElongationatBreak
%
ASTMD-638
23℃
>200
彎曲模數FlexuralModulus
kg/cm2
ASTMD-790A
23℃
9000
硬度Hardness
R-Scale
ASTMD-785
23℃
76
Izod衝擊強度IzodImpactStrength
kg-cm/cm
ASTMD-256
23℃1/8#39;#39;厚
23℃
N.B.
-20℃
8.3
熱變形溫度HeatDeflectionTemperature
℃
ASTMD-648at4.6kg/cm2
Unannealed1/4#39;#39;厚
98
收縮率MoldingShrinkage
%
FCFCMethod
23℃
1.4~1.8
比重SpecificGravity
ASTMD-792
23℃/23℃
0.90
FDACompliance
21CFR
Pt177.1520
Yes
UL94
AllColor
File:E162823
1/16"HB
Property | 單位Unit | 試驗方法TestMethod | 試驗條件TestCondition | K9017 | |
熔融指數MeltFlowIndex | g/10min | ASTMD-1238 | 230℃×2.16Kg | 17 | |
降伏點抗張強度TensileStrengthatYield |
kg/cm2 | ASTMD-638 | 23℃ | 210 | |
斷裂點延伸率TensileElongationatBreak | % | ASTMD-638 | 23℃ | >200 | |
彎曲模數FlexuralModulus | kg/cm2 | ASTMD-790A | 23℃ | 9000 | |
硬度Hardness | R-Scale | ASTMD-785 | 23℃ | 76 | |
Izod衝擊強度IzodImpactStrength | kg-cm/cm | ASTMD-256 | 23℃1/8#39;#39;厚 | 23℃ | N.B. |
-20℃ | 8.3 | ||||
熱變形溫度HeatDeflectionTemperature | ℃ | ASTMD-648at4.6kg/cm2 | Unannealed1/4#39;#39;厚 | 98 | |
收縮率MoldingShrinkage | % | FCFCMethod | 23℃ | 1.4~1.8 | |
比重SpecificGravity | ASTMD-792 | 23℃/23℃ | 0.90 | ||
FDACompliance | 21CFR Pt177.1520 |
Yes | |||
UL94 | AllColor | File:E162823 |