东莞市裕升高分子材料有限公司
357-BK1066
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
其它性能 | 热指数 | 电性能 | -- | UL 746B | 120 | deg C |
机械冲击性能 | -- | UL 746B | 120 | deg C | ||
非机械冲击性能 | -- | UL 746B | 140 | deg C | ||
物理性能 | 吸水率 | 24 小时 @ 73F | ASTM D-570 | 0.080 | % | |
比重 | 固体 | ASTM D-792 | 1.34 | --- | ||
比容 | --- | ASTM D-792 | 20.80 | in3/lb | ||
模塑收缩量 | 30-90 mil | flow | ASTM D-955 | 8-11 | in/in E-3 | |
90-180 mil | flow | ASTM D-955 | 10-14 | in/in E-3 | ||
30-90 mil | xflow | ASTM D-955 | 9-13 | in/in E-3 | ||
90-180 mil | xflow | ASTM D-955 | 12-16 | in/in E-3 | ||
机械性能 | 剪切强度 | --- | ASTM D-732 | 6000 | psi | |
挠曲模量 | --- | ASTM D-790 | 300000 | psi | ||
伊佐德冲击值 | 无缺口 | 73F | ASTM D-4812 | 60.0 | ft-lb/in | |
缺口 | 73F | ASTM D-256 | 10.0 | ft-lb/in | ||
修正加德纳冲击值 | --- | ASTM D-3029 | 32 | ft-lbs | ||
拉伸伸长 | 断裂 | ASTM D-638 | 110.0 | % | ||
加德纳冲击值 | --- | ASTM D-3029 | 32 | ft-lbs | ||
洛氏硬度 | --- | ASTM D-785 | 117 | R | ||
抗拉强度 | 屈服 | --- | ASTM D-638 | 7000 | psi | |
断裂 | --- | ASTM D-638 | 7000 | psi | ||
挠曲强度 | 屈服 | --- | ASTM D-790 | 12000 | psi | |
断裂 | --- | ASTM D-790 | 12000 | psi | ||
压缩强度 | --- | ASTM D-695 | 5300 | psi | ||
电气性能 | 介电强度 | 125 mils | 空气中 | ASTM D-149 | 470 | V/mil |
62 mils | 油内 | ASTM D-149 | 640 | V/mil | ||
125 mil | 油内 | ASTM D-149 | 470 | V/mil | ||
介电常数 | 100 Hz | -- | ASTM D-150 | 3.20 | -- | |
1 MHz | -- | ASTM D-150 | 3.20 | -- | ||
体积电阻率 | --- | ASTM D-257 | 1E16 | ohm-cm | ||
损耗因数 | 100 Hz | -- | ASTM D-150 | 0.0030 | -- | |
1 MHz | -- | ASTM D-150 | 0.0030 | -- | ||
加工性能 | CSA | --- | CSA LISTED | LS88480 | 文档号 | |
V-0额定值 (测试厚度) | --- | UL 94 | 0.025 | inch | ||
5VA额定值 (测试厚度) | --- | UL 94 | 0.120 | inch | ||
氧指数 (LOI) | --- | ASTM D-2863 | 30.0 | % | ||
UL文件号, 美国 | --- | --- | E121562 | --- | ||
热性能 | CTE(热膨胀系数) | -40F ~ 100F | flow | ASTM E-831 | 5 E-5 | in/in-F |
140F ~ 280F | flow | ASTM E-831 | 6 E-5 | in/in-F | ||
HDT(热畸变温度) | 未退火 | 66 psi | ASTM D-648 | deg F | 280 | |
未退火 | 264 psi | ASTM D-648 | deg F | 210 |