Ultramid 8232G HS FR BK102
聚酰胺6
产品说明:
Ultramid 8232G HS FR BK102 is a 25% glass fiber reinforced, heat stabilized, flame retardant pigmented black PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retardant ability with an excellent balance of high strength, stiffness and heat distortion temperature.
Applications
Ultramid 8232G HS FR BK102 is generally recommended for applications such as connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housings.
Applications
Ultramid 8232G HS FR BK102 is generally recommended for applications such as connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housings.
填料/增强材料
|
|
添加剂
|
|
特性
|
高刚性高强度较高的熔体稳定性热稳定性阻燃性 |
用途
|
家电部件开关连接器外壳线轴 |
机构评级
|
|
RoHS 合规性
|
|
外观
|
|
形式
|
|
加工方法
|
|
物理性能 |
额定值
|
单位制
|
测试方法
|
密度 / 比重
|
1.67
|
g/cm3
|
ASTM D792, ISO 1183 |
收缩率 - 流动 (3.18 mm)
|
0.30
|
%
|
|
吸水率
|
|||
饱和
|
4.0
|
%
|
ASTM D570 |
饱和, 23°C
|
4.0
|
%
|
ISO 62 |
平衡, 50% RH
|
1.1
|
%
|
ASTM D570 |
平衡, 23°C, 50% RH
|
1.1
|
%
|
ISO 62 |
硬度 |
额定值
|
单位制
|
测试方法
|
洛氏硬度 (R 级)
|
121
|
|
ASTM D785 |
机械性能 |
额定值
|
单位制
|
测试方法
|
拉伸模量 (23°C)
|
11000
|
MPa
|
ISO 527-2 |
抗张强度 (断裂, 23°C)
|
150
|
MPa
|
ASTM D638, ISO 527-2 |
伸长率 (断裂, 23°C)
|
1.9
|
%
|
ASTM D638, ISO 527-2 |
弯曲模量 (23°C)
|
10400
|
MPa
|
ASTM D790, ISO 178 |
冲击性能 |
额定值
|
单位制
|
测试方法
|
简支梁缺口冲击强度
|
ISO 179 | ||
-30°C
|
8.0
|
kJ/m2
|
|
23°C
|
9.4
|
kJ/m2
|
|
简支梁无缺口冲击强度 (23°C)
|
50
|
kJ/m2
|
ISO 179 |
悬壁梁缺口冲击强度
|
|||
23°C
|
77
|
J/m
|
ASTM D256 |
23°C
|
9.8
|
kJ/m2
|
ISO 180 |