性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 水吸收性 | 24h | ASTM D-570 | 0.4 | % |
透明性 | 3.2mm | ASTM D-1003 | 90 | % | |
比重 | ASTM D-792 | 1.16 | |||
反射指数 | ASTM D-542 | 1.49 | |||
机械性能 | 冲击强度 | Izod Notched | ASTM D-256 | 6.0 | kg·cm/cm2 |
洛氏硬度 | ASTM D-785 | 55 | M-Scale | ||
拉力 | ASTM D-638 | 450 | Kg/cm2 | ||
弯曲模数 | ASTM D-785 | 21,000 | Kg/cm2 | ||
弯曲强度 | ASTM D-790 | 800 | Kg/cm2 | ||
延伸率 | ASTM D-638 | 40 | % | ||
电气性能 | 介电强度 | 4KV/S | ASTM D-149 | 15 | KV/mm |
介电定数 | 60Hz | ASTM D-150 | 3.9 | ||
功率系数 | 60Hz | ASTM D-150 | 0.04 | ||
抗体积系数 | ASTM D-257 | >1515 | Ω.m | ||
热性能 | 绵性膨胀系数 | ASTM D-696 | 6×10-5 | cm/cm/°C | |
流动指数 | 230°C,3.8kg | ASTM D-1238 | 4.0 | g/10min | |
热变形温度 | 18.56kg | ASTM D-648 | 88 | °C | |
燃烧度 | 1/8",1/16" | UL94 | HB | ||
热传导 | ASTM D-177 | 5×10-4 | cal/seccm·°C/cm | ||
维卡软化点 | 1kg | ASTM D-1525 | 90 | °C | |
模缩系数 | ASTM D995-51 | 0.4-0.8 | % | ||
比热 | 0.35 | cal/g/°C |