艾博(国际)塑胶进出口有限公司
Notes: | Terluran® GP-35 is high-flow, general purpose injection molding grade with good ductility, intended for moldings with thin walls and/or adverse flow length to wall ratio. Excellent colorability, High flowability, Good impact resistance, Good heat distortion resistance, High quality surface finish and gloss, Great mechanical strength and rigidity. Applications: Injection molding, Thin wall components for telecommunications, Household and sanitary appliances, Toys, Automotive components, Electroplating. |
Vendors: | No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 g/cc | 0.0376 lb/in3 | ISO 1183 |
Moisture Absorption at Equilibrium | 0.24 % @Temperature 23.0 °C |
0.24 % @Temperature 73.4 °F |
50% RH; ISO 62 |
Water Absorption at Saturation | 0.95 % @Temperature 23.0 °C |
0.95 % @Temperature 73.4 °F |
ISO 62 |
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | ISO 294-4 |
Melt Flow | 34 g/10 min @Load 10.0 kg, Temperature 220 °C |
34 g/10 min @Load 22.0 lb, Temperature 428 °F |
Volumetric; cm3/10 min; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
Hardness, Rockwell R | 102 | 102 | ASTM Test |
Ball Indentation Hardness | 99.0 MPa | 14400 psi | ISO 2039-1 |
Tensile Strength, Yield | 44.0 MPa | 6380 psi | ISO 527 |
Elongation at Break | 12 % | 12 % | Nominal; ISO 527 |
>= 15.0 % | >= 15.0 % | ISO 527 | |
Elongation at Yield | 2.4 % | 2.4 % | ISO 527 |
Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527 |
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM Test |
0.850 J/cm @Temperature -18.0 °C |
1.59 ft-lb/in @Temperature -0.400 °F |
ASTM Test |