艾博(国际)塑胶进出口有限公司现货供应 ExxonMobil Escorene LD-333 EVA Film,原产原包,可随货提供原材料物性,COA,SGS.MSDS.UL黄卡等相关详细资料,欢迎来人来电咨讯
ExxonMobil Escorene LD-333 EVA Film
Physical Properties |
Metric |
English |
Comments |
Density |
0.930 g/cc |
0.0336 lb/in3 |
Exxon Method |
Thickness |
31.8 microns |
1.25 mil |
|
Melt Flow |
0.90 g/10 min |
0.90 g/10 min |
Exxon Method |
|
Mechanical Properties |
Metric |
English |
Comments |
Film Tensile Strength at Yield, MD |
7.60 MPa |
1100 psi |
ASTM D882 |
Film Tensile Strength at Yield, TD |
6.20 MPa |
899 psi |
ASTM D882 |
Film Elongation at Break, MD |
230 % |
230 % |
ASTM D882 |
Film Elongation at Break, TD |
635 % |
635 % |
ASTM D882 |
Secant Modulus, MD |
0.130 GPa |
18.9 ksi |
ASTM D882 |
Secant Modulus, TD |
0.160 GPa |
23.2 ksi |
ASTM D882 |
Elmendorf Tear Strength MD |
110 g |
110 g |
ASTM D1922 |
Elmendorf Tear Strength TD |
70 g |
70 g |
ASTM D1922 |
Elmendorf Tear Strength, MD |
3.46 g/micron |
88.0 g/mil |
ASTM D1922 |
Elmendorf Tear Strength, TD |
2.20 g/micron |
56.0 g/mil |
ASTM D1922 |
Dart Drop |
7.87 g/micron |
200 g/mil |
F50; ASTM D1709 |
Dart Drop Test |
250 g |
0.551 lb |
F50; ASTM D-1709 |
Film Tensile Strength at Break, MD |
37.0 MPa |
5370 psi |
ASTM D882 |
Film Tensile Strength at Break, TD |
28.0 MPa |
4060 psi |
ASTM D882 |
|
|
|
|
|
由制造商提供的数据,埃克森美孚化工。
A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.
9%醋酸乙烯酯共聚物膜树脂。由ld-333膜表现出优异的冲击强度,透明度和热封性。
Applications: Primal meat bags; Retail meat packages; Cheese packaging. Data for film properties below based on 1.25 mil film.
应用:原始的肉袋;肉类零售包装的奶酪包装。膜的性能,在基于1.25 mil电影数据
现货供应全系列产品可随货提供原材料物性,原材料产地证明SGS.MSDS.UL黄卡等相关详细资料,可开具17%增值税发票.公司秉着“以诚为本,以信为用”的经营理念。与客户是建立在互惠、互利、互信的基础上长期合作。共创双赢局面,愿与各界人士真诚合作,共同发展,携手共创辉煌的明天。 |