艾博(国际)塑胶进出口有限公司现货供应 ExxonMobil EXACT 8201 Plastomer,原产原包,可随货提供原材料物性,COA,SGS.MSDS.UL黄卡等相关详细资料,欢迎来人来电咨讯
ExxonMobil EXACT 8201 Plastomer
乙烯-辛烯共聚物使用埃克森美孚化工EXXPOL技术生产。设计用于单层和多层工业吹塑薄膜的应用需要突出的低温密封性能。
Physical Properties |
Metric |
English |
Comments |
Density |
0.882 g/cc |
0.0319 lb/in3 |
ExxonMobil Method |
Thickness |
31.8 microns |
1.25 mil |
|
Melt Flow |
1.1 g/10 min |
1.1 g/10 min |
ExxonMobil Method |
|
Mechanical Properties |
Metric |
English |
Comments |
Film Tensile Strength at Yield, MD |
4.14 MPa |
600 psi |
2% Offset; ASTM D882 |
Film Tensile Strength at Yield, TD |
2.76 MPa |
400 psi |
2% Offset; ASTM D882 |
Film Elongation at Break, MD |
390 % |
390 % |
ASTM D882 |
Film Elongation at Break, TD |
720 % |
720 % |
ASTM D882 |
Film Elongation at Yield, MD |
15.2 % |
15.2 % |
ASTM D882 |
Film Elongation at Yield, TD |
10.2 % |
10.2 % |
ASTM D882 |
Puncture Energy |
9.60 J |
7.08 ft-lb |
ExxonMobil Method |
Elmendorf Tear Strength, MD |
1.10 g/micron |
28.0 g/mil |
ASTM D1922 |
Elmendorf Tear Strength, TD |
4.72 g/micron |
120 g/mil |
ASTM D1922 |
Dart Drop |
8.50 g/micron |
216 g/mil |
ASTM D1709A |
Film Tensile Strength at Break, MD |
66.3 MPa |
9620 psi |
ASTM D882 |
Film Tensile Strength at Break, TD |
|
|
现货供应全系列产品可随货提供原材料物性,原材料产地证明SGS.MSDS.UL黄卡等相关详细资料,可开具17%增值税发票.公司秉着“以诚为本,以信为用”的经营理念。与客户是建立在互惠、互利、互信的基础上长期合作。共创双赢局面,愿与各界人士真诚合作,共同发展,携手共创辉煌的明天。 |